Nordiska Amalgam ANA 70 (Wykle Research)
Nordiska amalgams are superior in many quality aspects. They have well balanced expansion and high strength. This combination gives tight margins, long lasting fillings and few marginal breakdowns.
- High silver
- Spherical
- Silver shining
- Soft condensation feeling
- Alloy composition: Ag 69.9%, Sn 18.8%, Cu 10.2%, Zn 1.1%
- Compressive strength: 1h - 10 MPa, 24h - 420 MPa, 7 days - 480 MPa
- Static creep: 1%
- Dimensional change: 24h +0.1%
ANA 70 CAPSULES
- No. 1 – Gold capsule (400 mg alloy + 430 mg mercury)
- No. 2 – Orange capsule (600 mg alloy + 640 mg mercury)
- No. 3 – Purple capsule (800 mg alloy + 860 mg mercury)
Nordiska amalgams are superior in many quality aspects. They have well balanced expansion and high strength. This combination gives tight margins, long lasting fillings and few marginal breakdowns.
- High silver
- Spherical
- Silver shining
- Soft condensation feeling
- Alloy composition: Ag 69.9%, Sn 18.8%, Cu 10.2%, Zn 1.1%
- Compressive strength: 1h - 10 MPa, 24h - 420 MPa, 7 days - 480 MPa
- Static creep: 1%
- Dimensional change: 24h +0.1%
ANA 70 CAPSULES
- No. 1 – Gold capsule (400 mg alloy + 430 mg mercury)
- No. 2 – Orange capsule (600 mg alloy + 640 mg mercury)
- No. 3 – Purple capsule (800 mg alloy + 860 mg mercury)
Delivery
All orders shipped with UPS Express.
Always free shipping for orders over US $250.
All orders are shipped with a UPS tracking number.
Returns
Items returned within 14 days of their original shipment date in same as new condition will be eligible for a full refund or store credit.
Refunds will be charged back to the original form of payment used for purchase.
Customer is responsible for shipping charges when making returns and shipping/handling fees of original purchase is non-refundable.
All sale items are final purchases.
Help
Give us a shout if you have any other questions and/or concerns.
Email: contact@domain.com
Phone: +1 (23) 456 789
Nordiska amalgams are superior in many quality aspects. They have well balanced expansion and high strength. This combination gives tight margins, long lasting fillings and few marginal breakdowns.
- High silver
- Spherical
- Silver shining
- Soft condensation feeling
- Alloy composition: Ag 69.9%, Sn 18.8%, Cu 10.2%, Zn 1.1%
- Compressive strength: 1h - 10 MPa, 24h - 420 MPa, 7 days - 480 MPa
- Static creep: 1%
- Dimensional change: 24h +0.1%
ANA 70 CAPSULES
- No. 1 – Gold capsule (400 mg alloy + 430 mg mercury)
- No. 2 – Orange capsule (600 mg alloy + 640 mg mercury)
- No. 3 – Purple capsule (800 mg alloy + 860 mg mercury)